China factories

China factory - Xi'an Huance Automation Technology Co., Ltd.

Xi'an Huance Automation Technology Co., Ltd.

  • China,Yantai ,Shandong
  • Active Member

Leave a Message

we will call you back quickly!

Submit Requirement
China Weld Cracks Internal Ultrasonic Flaw Detector Nondestructive
China Weld Cracks Internal Ultrasonic Flaw Detector Nondestructive

  1. China Weld Cracks Internal Ultrasonic Flaw Detector Nondestructive
  2. China Weld Cracks Internal Ultrasonic Flaw Detector Nondestructive
  3. China Weld Cracks Internal Ultrasonic Flaw Detector Nondestructive

Weld Cracks Internal Ultrasonic Flaw Detector Nondestructive

  1. MOQ: 1
  2. Price:
  3. Get Latest Price
Payment Terms L/C, D/A, D/P, T/T, Western Union, MoneyGram
Supply Ability PIECE/WEEK
Delivery Time 3 to 7 working days after payment
Packaging Details Carton
Detection sensitivity margin 60dB
Display screen Display: high-brightness color flat panel display
Power Adapter Input 100V ~ 240V/50Hz ~ 60Hz output 9V/1.5A
Brand Name HCATM
Model Number HU800
Place of Origin XIAN

View Detail Information

Contact Now Ask for best deal
Get Latest Price Request a quote
  1. Product Details
  2. Company Details

Product Specification

Payment Terms L/C, D/A, D/P, T/T, Western Union, MoneyGram Supply Ability PIECE/WEEK
Delivery Time 3 to 7 working days after payment Packaging Details Carton
Detection sensitivity margin 60dB Display screen Display: high-brightness color flat panel display
Power Adapter Input 100V ~ 240V/50Hz ~ 60Hz output 9V/1.5A Brand Name HCATM
Model Number HU800 Place of Origin XIAN
High Light Weld Cracks Ultrasonic Flaw DetectorInternal Ultrasonic Flaw Detector60dB Ultrasonic Flaw Detector

Digital ultrasonic flaw detector

Metal ultrasonic flaw detector is a portable industrial non-destructive flaw detection instrument, which can quickly, conveniently, damage-free and accurately detect and locate various defects in the workpiece (including longitudinal cracks, transverse cracks, looseness, pores, slag inclusions, etc.) , Evaluation and diagnosis. It can be used both in the laboratory and on the engineering site.

 

Instrument application
Widely used in boilers, pressure vessels, aerospace, aviation, electric power, petroleum, chemical, offshore oil, pipelines, military industry, shipbuilding, automobiles, machinery manufacturing, metallurgy, metal processing industry, steel structure, railway transportation, nuclear power, universities, etc. industry.

 

Instrument principle
When the ultrasonic wave propagates in the material to be tested, the acoustic properties of the material and the change of the internal organization have a certain influence on the propagation of the ultrasonic wave. The technology of understanding the material performance and structural changes through the detection of the degree and condition of the ultrasonic wave is called ultrasonic testing. Ultrasonic testing methods usually include penetration method, pulse reflection method, tandem method and so on.

 

Technical Parameters

Name Technical data
Scanning range (mm)

0 ~ 10000 steps: 2.5, 5, 10, 20, 30, 40, 50, 60, 70, 80, 90, 100, 150, 200, 250, 300, 350, 400,

450, 500, 600, 700, 800, 900, 1000, 2000, 3000, 4000, 5000, 6000, 7000, 8000, 9000, 10000. Adjustment step: 1mm

Pulse shift (s)

Pulse shift (s): -20 ~ +3400

Gear levels: -20,- 10,0.0, 10, 20, 50,100,150,200,250,300,350,400,450,500, 600,700,800,900,1000, 1500,2000,2500,3000,3400. Adjustment step: 0.1 (-20 s ~ 999.9 s), 1 (1000 s ~ 3400s)

Probe zero point (s)

Probe zero point: 0.0 ~ 99.99 adjustment step: 0.01

Material sound velocity: 1000~15000

Material sound velocity (m/s)

7 fixed sound speeds: 2260, 2730, 3080, 3230, 4700, 5900, 6300

Adjustment step: 1

Way of working Single probe (receiving, sending), double probe (one receiving--sending)
Frequency range (MHz) Broadband 0.5-20
Gain adjustment (dB) 0~130 adjustment step: 1, 2, 6, 12
Linear suppression 0% ~ 80% of screen height, step distance: 1%
Vertical linearity error Vertical linear error is not more than 3%
Horizontal linearity error Within the scanning range, no more than 0.2%
Detection sensitivity margin 60dB
Dynamic Range 32dB
Call the police Incoming wave alarm
Display screen Display: high-brightness color flat panel display
A- Scan display area Full screen or partial A-Scan display freeze and unfreeze A-Scan fill
Flaw detection channel 500 pcs
data storage 100 A-Scan graphics
Communication interface standard with PC USB
Units of measurement. Mm
Power Adapter Input 100V ~ 240V/50Hz ~ 60Hz output 9V/1.5A
battery Lithium battery 5000mAh
Working temperature (°C) -10 ~ 50

 

Important auxiliary functions

●Two input methods of angle and K value
●Analysis of the number of echoes
●Power status indication
●Gate] Sound and light alarm
●DAC sound and light alarm
●Freezing and thawing of screen
●Clock display
●Hibernation and screen saver

 

Product details digital ultrasonic flaw detector

 

Mode of transport

Company Details

Bronze Gleitlager

,

Bronze Sleeve Bushings

 and 

Graphite Plugged Bushings

 from Quality China Factory
  • Business Type:

    Manufacturer

  • Year Established:

    2007

  • Total Annual:

    8000000-10000000

  • Employee Number:

    80~120

  • Ecer Certification:

    Active Member

  Xi'an Huance Automation Technology Co., Ltd. is located in Xi'an High-tech Development Zone - Free Trade Zone, China, was established in 2007. Huance specializes in the research and development of liquid ultrasonic flowmeter, gas ultrasonic flowmeter, Coriolis mass flowme...   Xi'an Huance Automation Technology Co., Ltd. is located in Xi'an High-tech Development Zone - Free Trade Zone, China, was established in 2007. Huance specializes in the research and development of liquid ultrasonic flowmeter, gas ultrasonic flowmeter, Coriolis mass flowme...

+ Read More

Get in touch with us

  • Reach Us
  • Xi'an Huance Automation Technology Co., Ltd.
  • Room 11206, Unit 1, Building 2, Green Square, Jinye Road, Zhangba Street, Yantai District, Xi'an
  • https://www.pressureflowmeter.com/

Leave a Message, we will call you back quickly!

Email

Check your email

Phone Number

Check your phone number

Requirement Details

Your message must be between 20-3,000 characters!

Submit Requirement