| Payment Terms | L/C, T/T |
| Supply Ability | 200 tons per year |
| Delivery Time | 6-8 weeks |
| Packaging Details | In bundles in woode box |
| Similar Grade | GH3536, GH536,GH22, GH334, GH739, SG-5, UNS N06002, NC22FeD, NiCr22FeMo, Nimonic PE13 |
| Material | Hastelloy C |
| Application | Used in the manufacture of aircraft engine combustion chamber components and other high temperature components |
| Density | 8.28g/cm³ |
| Melting temperature | 1295℃-1381℃ |
| Brand Name | Torich |
| Model Number | Alloy Steel Pipe HastelloyX |
| Certification | CE PED |
| Place of Origin | China |
View Detail Information
Explore similar products
Copper / Copper Alloy Condenser Seamless Steel Tube 10 - 80mm OD ASTM B111
Titanium Welded Seamless Alloy Steel Pipe TA3 TA9 TA10 0.5 - 2mm Wall Thickness
Automobile High Carbon Chromium 100cr6 Bearing Tube 16MnCr5
Astmb338 Coll Roll Titanium Alloy Tube For Heat Exchangers / Condensers
Product Specification
| Payment Terms | L/C, T/T | Supply Ability | 200 tons per year |
| Delivery Time | 6-8 weeks | Packaging Details | In bundles in woode box |
| Similar Grade | GH3536, GH536,GH22, GH334, GH739, SG-5, UNS N06002, NC22FeD, NiCr22FeMo, Nimonic PE13 | Material | Hastelloy C |
| Application | Used in the manufacture of aircraft engine combustion chamber components and other high temperature components | Density | 8.28g/cm³ |
| Melting temperature | 1295℃-1381℃ | Brand Name | Torich |
| Model Number | Alloy Steel Pipe HastelloyX | Certification | CE PED |
| Place of Origin | China | ||
| High Light | alloy steel seamless tube ,seamless alloy steel pipe | ||
Alloy Steel Pipe HastelloyX
Hastelloy X is a kind of nickel-based superalloy with high iron content, which is mainly solution strengthened by chromium and molybdenum solution strengthening. It has good resistance to oxidation and corrosion resistance. It has good cold & hot formability and weldability because its moderate lasting and creep strength under 900℃. Used in the manufacture of aircraft engine combustion chamber components and other high temperature components. It can be long-term used under 900℃, and short-term working temperature can up to 1080℃.
Similar Grade of Hastelloy X: GH3536, GH536,GH22, GH334, GH739, SG-5, UNS N06002, NC22FeD, NiCr22FeMo, Nimonic PE13, Hastelloy H
Application for Hastelloy X: Used in the manufacture of aircraft engine combustion chamber components and other high temperature components
Chemical Composition of Hastelloy X:
| Chemical Composition (%) | ||||||||||||||
| C | Cr | Ni | Co | W | Mo | Al | Ti | Fe | B | Cu | Mn | Si | P | S |
| 0.05-0.15 | 20.5-23.0 | Margin | 0.50-2.50 | 0.20-1.00 | 8.0- 10.0 | ≤0.50 | ≤0.15 | 17.0-20.0 | ≤0.010 | ≤0.5 | ≤1.00 | ≤1.00 | ≤0.025 | ≤0.015 |
Hastelloy X Physical Properties:
Hastelloy X Density: ρ: 8.28g/cm³
Hastelloy X Melting Temperature Rage: 1295℃-1381℃
Coefficient of Thermal Conductivity of Hastelloy X:
| coefficient of thermal conductivity | |||||||||
| Temperature ℃ | 100 | 200 | 300 | 400 | 500 | 600 | 700 | 800 | 900 |
| λ/(w/(m.℃)) | 13.38 | 17.97 | 20.27 | 22.4 | 24.62 | 26.79 | 29.05 | 31.14 | 33.44 |
Specific Heat Capacity for Hastelloy X:
| Specific Heat Capacity | ||||||||||
| Temperature ℃ | 17 | 100 | 200 | 300 | 400 | 500 | 600 | 700 | 800 | 900 |
| C/J/( kg · K ) | 372.6 | 372.6 | 389.4 | 456.4 | 427.1 | 452.2 | 464.7 | 515 | 535.9 | 561 |
Expansion Coefficient for Hastelloy X:
| expansion coefficient | |||||||||
| Temperature/℃ | 20-100 | 20-200 | 20-300 | 20-400 | 20-500 | 20-600 | 20-700 | 20-800 | 20-900 |
| α1/10-6℃-1 | 12.1 | 12.5 | 13.4 | 14 | 14.3 | 14.8 | 15.5 | 15.8 | 16.1 |
Resistivity of Hastelloy X:
| resistivity | |||||||||
| Temperature/℃ | 100 | 200 | 300 | 400 | 500 | 600 | 700 | 800 | 900 |
| Resistor Ω·m | 1.18 | 1.2 | 1.21 | 1.22 | 1.24 | 1.25 | 1.26 | 1.27 | 1.29 |
Hastelloy X is widely used in aircraft engine and the civilian industry in adroad, and in our country, it mainly used in the manufacture of hot end of combustion chamber parts and other components, and honeycomb structure, etc. Besides, long-term used at high temperature will have certain age hardening phenomenon.
![]()
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Importer,Exporter,Trading Company,Seller
Year Established:
1997
Total Annual:
25000000-30000000
Employee Number:
100~200
Ecer Certification:
Verified Supplier
Who We are ? -------A professional steel pipes materials inventor, manufacturer and solution providerTorich International Limited is a professional manufacturer and exporter of steel pipes materials. It is an international marketing and sales company specialized in steel tubes, which holds the ... Who We are ? -------A professional steel pipes materials inventor, manufacturer and solution providerTorich International Limited is a professional manufacturer and exporter of steel pipes materials. It is an international marketing and sales company specialized in steel tubes, which holds the ...
Get in touch with us
Leave a Message, we will call you back quickly!