Packaging Details | wooden box |
Delivery Time | 15-20 days |
Payment Terms | T/T L/C |
Supply Ability | 100000KG/MONTH |
Delivery State | Sosoloid |
Features | Fatigue Resistance, Radiation Resistance, Oxidation Resistance, Corrosion Resistance |
Alloy Type | Nickel-based Deformed Superalloy |
Application | Parts For Aero-engine, Nuclear Energy Industry And Petroleum Applications |
Shape | Wire,Strip,Rod,Pipe,Plate |
Executive standard | ASTM |
Size | Negotiable |
Raw Materials | NI50-55%, CR17-21%, NB4.75-5.5%, MO2.8-3.3% |
Brand Name | KAIXIN |
Model Number | inconel 600 |
Place of Origin | China |
Certification | ISO9001:2005 |
View Detail Information
Explore similar products
Inconel 738 Round Bar Tube Sheet Nickel Alloy Wire
GH4145 Nickel Based Welding Wire Inconel 750 Round Bar Tube Sheet
Oxidation Resistance Inconel 600 Round Bar Alloy 600 Sheet Inconel 600 Tube
NS313 Alloy 601 Round Bar ASTM Nickel Alloy Wire Inconel Tube Inconel Sheet
Product Specification
Packaging Details | wooden box | Delivery Time | 15-20 days |
Payment Terms | T/T L/C | Supply Ability | 100000KG/MONTH |
Delivery State | Sosoloid | Features | Fatigue Resistance, Radiation Resistance, Oxidation Resistance, Corrosion Resistance |
Alloy Type | Nickel-based Deformed Superalloy | Application | Parts For Aero-engine, Nuclear Energy Industry And Petroleum Applications |
Shape | Wire,Strip,Rod,Pipe,Plate | Executive standard | ASTM |
Size | Negotiable | Raw Materials | NI50-55%, CR17-21%, NB4.75-5.5%, MO2.8-3.3% |
Brand Name | KAIXIN | Model Number | inconel 600 |
Place of Origin | China | Certification | ISO9001:2005 |
High Light | 600 Inconel Alloy ,Nickel Based Deformed Superalloy ,ASTM Standard Inconel Alloy |
Inconel 625 is a nickel-based deformed superalloy that has superior fatigue resistance, radiation resistance, oxidation resistance, and corrosion resistance. It is an ideal choice for parts that are used in aero-engine, nuclear energy industry, and petroleum applications. It is available in a variety of shapes such as wire, strip, rod, pipe, and plate, and the size can be customized according to the customer’s requirements. Inconel 625 is capable of withstanding extreme temperatures and high pressures. It also has excellent weldability and can be easily machined to the desired shape. It is an ideal material for components that require superior mechanical properties and corrosion resistance.
Property | Description |
---|---|
Alloy Type | Nickel-based Deformed Superalloy |
Features | Fatigue Resistance, Radiation Resistance, Oxidation Resistance, Corrosion Resistance |
Size | Negotiable |
Raw Materials | NI50-55%, CR17-21%, NB4.75-5.5%, MO2.8-3.3% |
Shape | Wire,Strip,Rod,Pipe,Plate |
Application | Parts For Aero-engine, Nuclear Energy Industry And Petroleum Applications |
Executive standard | ASTM |
Delivery State | Solid |
AWSA5.14:2005 alloy 625 | Nr.2.4856 |
Inconel Alloy, also known as UNS N06625 or Alloy 625, is a nickel-chromium-molybdenum alloy with high strength and excellent corrosion resistance. It is used in a variety of industrial applications, such as aircraft parts, chemical processing, power plants, and nuclear reactors. KAIXIN's Inconel 600 has been certified by ISO9001:2005 and its raw materials include NI50-55%, CR17-21%, NB4.75-5.5%, MO2.8-3.3%. The executive standard is ASTM and the delivery state is sosoloid. It is available in various shapes, such as wire, strip, rod, pipe, and plate. The size is negotiable and the minimum order quantity is 30kg. The price range is between 50-52 USD/kg and the delivery time is 15-20 days. The payment terms are T/T or L/C and the supply ability is 100000KG/MONTH. Packaging is provided in wooden boxes.
Inconel Alloy provides technical support and service to its customers. Customers can contact the technical support team via phone, email or online chat. The team is available 24/7 to help with any queries that may arise. Additionally, the company provides online resources including technical documents, videos, tutorials and forums. All these resources can be accessed to provide customers with the information they need to get the most out of their Inconel Alloy products.
Company Details
Business Type:
Manufacturer,Trading Company
Year Established:
2007
Total Annual:
10000000-30000000
Employee Number:
150~200
Ecer Certification:
Verified Supplier
Danyang Kaixin Alloy Materials Co., Ltd. was founded on April 18th, 2007, covering an area of 13500 square meters with a registered capital of 20 million yuan. It is a professional enterprise engaged in independent production,research and development of high performance alloy materials such as preci... Danyang Kaixin Alloy Materials Co., Ltd. was founded on April 18th, 2007, covering an area of 13500 square meters with a registered capital of 20 million yuan. It is a professional enterprise engaged in independent production,research and development of high performance alloy materials such as preci...
Get in touch with us
Leave a Message, we will call you back quickly!