Name | Nickel Based Superalloy |
Density | ~8.6 g/cm³ (0.310 lb/in³) |
Melting Point | ~1300-1400°C (2370-2550°F) |
Tensile Strength | ~950 MPa (138 ksi) |
Yield Strength | ~750 MPa (109 ksi) |
Elongation | ~15% |
Thermal Conductivity | ~12 W/m·K (8.4 BTU·in/hr·ft²·°F) |
Modulus of Elasticity | ~210 GPa (30 x 10³ ksi) |
Corrosion Resistance | Good oxidation and corrosion resistance at high temperatures |
Applications | Aerospace components, gas turbines, high-temperature structural parts |
Brand Name | Zhonggong Special Metallurgy |
Model Number | GH132 Alloy |
Place of Origin | China |
Certification | ISO Certificate |
View Detail Information
Explore similar products
Temperature Resistant Inconel 706 Nickel Based Alloys For Aerospace Components
High Strength Inconel 718 Rod Anti Deformation High Temperature Bolts / Nuts /
Good Weldability Nickel Based Alloys 625 UNS N06625 Customized Dimensions
Corrosion Resistant Nickel Based Alloy 926 For Extreme Industrial Environments
Product Specification
Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, | Supply Ability | 5000 tons per month |
Delivery Time | 5-8 working days, depending on the parameters required for negotiation | Packaging Details | Standard export packaging, or packaging as required |
Name | Nickel Based Superalloy | Density | ~8.6 g/cm³ (0.310 lb/in³) |
Melting Point | ~1300-1400°C (2370-2550°F) | Tensile Strength | ~950 MPa (138 ksi) |
Yield Strength | ~750 MPa (109 ksi) | Elongation | ~15% |
Thermal Conductivity | ~12 W/m·K (8.4 BTU·in/hr·ft²·°F) | Modulus of Elasticity | ~210 GPa (30 x 10³ ksi) |
Corrosion Resistance | Good oxidation and corrosion resistance at high temperatures | Applications | Aerospace components, gas turbines, high-temperature structural parts |
Brand Name | Zhonggong Special Metallurgy | Model Number | GH132 Alloy |
Place of Origin | China | Certification | ISO Certificate |
High Light | Nickel Based Superalloy Oxidation Resistant ,High Strength Nickel Based Superalloy |
GH132 Alloy Is A High-Strength Nickel-Based Superalloy With Excellent High-Temperature Stability And Oxidation Resistanc
GH132 Alloy is a high-performance nickel-based superalloy designed for demanding high-temperature applications. It is known for its exceptional strength and stability under elevated temperatures, making it ideal for use in aerospace and industrial environments.
Key Properties and Features:
GH132 Alloy’s superior performance in extreme conditions ensures it is a trusted choice for advanced engineering applications requiring high durability and reliability.
Here is a composition table for GH132 Alloy:
Element | Composition Range (%) |
---|---|
Nickel (Ni) | 60.0 - 65.0 |
Chromium (Cr) | 14.0 - 16.0 |
Cobalt (Co) | 8.0 - 10.0 |
Molybdenum (Mo) | 2.5 - 4.0 |
Iron (Fe) | ≤ 6.0 |
Titanium (Ti) | 1.0 - 2.0 |
Aluminum (Al) | 1.0 - 2.0 |
Carbon (C) | ≤ 0.10 |
Manganese (Mn) | ≤ 0.5 |
Silicon (Si) | ≤ 0.5 |
Sulfur (S) | ≤ 0.01 |
These values are general guidelines. For specific applications or precise compositions, consult with industry standards or suppliers.
Company Details
Business Type:
Manufacturer,Distributor/Wholesaler,Agent,Importer,Exporter,Seller,Other
Year Established:
2022
Total Annual:
1000000-1500000
Employee Number:
100~200
Ecer Certification:
Verified Supplier
Main Products Stainless Steel Series304,304L,321,316L,317L,309s,310s,904L,410,420,430,441,409,436,441,439,630 etc. Duplex stainless steel series 2205,2507 etc. Hastelloy C-276, B-2, C-2000, etc. Nickel-based alloy series Inconel625,718,Incoloy825,800H,Monel400, etc. High temperature alloy ser... Main Products Stainless Steel Series304,304L,321,316L,317L,309s,310s,904L,410,420,430,441,409,436,441,439,630 etc. Duplex stainless steel series 2205,2507 etc. Hastelloy C-276, B-2, C-2000, etc. Nickel-based alloy series Inconel625,718,Incoloy825,800H,Monel400, etc. High temperature alloy ser...
Get in touch with us
Leave a Message, we will call you back quickly!